Abstract
The samples of hydroxyapatite and carbonate substituted hydroxyapatite (CHA) were obtained under the influence of physical factors, namely ultrasound (US) and microwave (MW) radiations. The results of Fourier transform infrared spectroscopy and X-ray diffraction analysis have proved the formation of the calcium deficient hydroxyapatite and B-type CHA with the Ca/P ratio in the ranges 1.62-1.87. In vitro studies have showed the increased bioactivity of the samples, synthesized under the influence of physical factors as compared to the standard ones. The samples of both groups, synthesized under the influence of 600 W MW, have shown the greatest stability in biological environment. In vivo tests confirm that obtained under US and MW radiations hydroxyapatite-based biomaterials are biocompatible, non-toxic and exhibit osteoconductive properties. The usage of US and MW radiations can significantly shorten the time (up to 5-20 min) of obtaining of calcium deficient hydroxyapatite and B-type CHA in nanopowder form, close in structure and composition to the biological hydroxyapatite.
AI evidence extraction
Structured fields below were generated from the paper’s abstract and metadata to make the evidence easier to inspect. Automated extraction may be incomplete or incorrect; verify important details against the original paper.
Main findings
Hydroxyapatite and carbonate-substituted hydroxyapatite synthesized under ultrasound and microwave radiation formed calcium-deficient hydroxyapatite and B-type CHA (Ca/P 1.62–1.87). In vitro, samples synthesized under these physical factors showed increased bioactivity versus standard samples, and those synthesized under 600 W microwave showed the greatest stability in a biological environment. In vivo tests reported the materials as biocompatible, non-toxic, and osteoconductive, and the use of ultrasound/microwave shortened synthesis time to 5–20 minutes.
Outcomes measured
- Hydroxyapatite/CHA structural features (FTIR, XRD)
- Ca/P ratio
- In vitro bioactivity
- Stability in biological environment
- In vivo biocompatibility
- Toxicity
- Osteoconductive properties
- Synthesis time reduction
Limitations
- No microwave frequency or exposure characterization beyond power (600 W) is provided in the abstract
- No sample sizes or details of in vitro/in vivo methods are provided in the abstract
- This is a materials synthesis/bioactivity study rather than a study of EMF exposure effects on humans or animals
View raw extracted JSON
{
"study_type": "other",
"exposure": {
"band": null,
"source": "microwave radiation",
"frequency_mhz": null,
"sar_wkg": null,
"duration": "5-20 min (synthesis time mentioned)"
},
"population": null,
"sample_size": null,
"outcomes": [
"Hydroxyapatite/CHA structural features (FTIR, XRD)",
"Ca/P ratio",
"In vitro bioactivity",
"Stability in biological environment",
"In vivo biocompatibility",
"Toxicity",
"Osteoconductive properties",
"Synthesis time reduction"
],
"main_findings": "Hydroxyapatite and carbonate-substituted hydroxyapatite synthesized under ultrasound and microwave radiation formed calcium-deficient hydroxyapatite and B-type CHA (Ca/P 1.62–1.87). In vitro, samples synthesized under these physical factors showed increased bioactivity versus standard samples, and those synthesized under 600 W microwave showed the greatest stability in a biological environment. In vivo tests reported the materials as biocompatible, non-toxic, and osteoconductive, and the use of ultrasound/microwave shortened synthesis time to 5–20 minutes.",
"effect_direction": "unclear",
"limitations": [
"No microwave frequency or exposure characterization beyond power (600 W) is provided in the abstract",
"No sample sizes or details of in vitro/in vivo methods are provided in the abstract",
"This is a materials synthesis/bioactivity study rather than a study of EMF exposure effects on humans or animals"
],
"evidence_strength": "insufficient",
"confidence": 0.74,
"peer_reviewed_likely": "yes",
"keywords": [
"hydroxyapatite",
"carbonated apatite",
"carbonate substituted hydroxyapatite",
"ultrasound",
"microwave radiation",
"FTIR",
"X-ray diffraction",
"bioactivity",
"biocompatibility",
"osteoconductive",
"nanomaterials"
],
"suggested_hubs": []
}AI-extracted fields are generated from the abstract and metadata and may be incomplete or incorrect. This material is for informational purposes and is not medical advice.
Identifiers and source
DOI: 10.1016/j.ultsonch.2017.11.011
PubMed: 29429738
Related papers
- Nanocrystalline hydroxyapatite bioceramic using microwave radiation: Synthesis and characterization. 2010
- Hydrogel-hydroxyapatite-monomeric collagen type-I scaffold with low-frequency electromagnetic field treatment enhances osteochondral repair in rabbits. 2021
- Highly biocompatible, nanocrystalline hydroxyapatite synthesized in a solvothermal process driven by high energy density microwave radiation. 2013
- Cellular signaling pathways in the nervous system activated by various mechanical and 2024
- RF-EMF Exposure Assessment of Fetus During The First Trimester of Pregnancy 2024
- Where is your smartphone? An unusual mass within the tensor fasciae latae muscle 2023